i am looking ASME VIII div1 , requirement same above as per project specification below details , I am looking for <19mm 
P1 through P5B materials with wall thickness  19 mm (0.75 in.) shall only be
interrupted provided a minimum of 10 mm (0.375 in.) of weld metal has been deposited or 25 percent of the weld
groove has been filled, whichever is greater. If welding is interrupted, the weld shall be covered with adequate
insulation to ensure slow cooling. The partially completed weld shall be 100 percent MT-inspected prior to
resuming welding.

On Thu, Apr 1, 2021 at 1:33 PM mahesh chilukamari <chilukamarimahesh@gmail.com> wrote:
Hi,
Refer to below from ASME B31.1


On Thu, 1 Apr 2021 at 2:51 PM, sankar krishnan <sankar.bombay@gmail.com> wrote:
Dear All ,

  In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thickness 

Please send me code documents 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ca6ac61-bff9-444e-bc40-80249c545c8dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOgMkxFmV3eyTp9POam51Aonan%2BAau%2B%3DkiBO5cYQ%2BqYLWE%3DQcw%40mail.gmail.com.


--
shankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyDEeabiVagTQhzbsS6p-1VVVuMHv9Xjy5JEsxEYuVbZUDN%2BQ%40mail.gmail.com.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone