Dear friends,

I would  like to know about salt spray test method for valves . can you give me details of test ? how it was carried out ? what standard to follow ? How many hours to carry out this test ? expect your reply with details. 

 

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material