Monday, April 5, 2021

[MW:32162] Any Special requirements of welder qualification for weld cladding materials?

Dear Experts,

Any Special requirements of welder qualification for weld cladding materials?

(Stainless steel, copper alloys & Nickel based alloys)

Please explain Sec-IX and reference.

Thanks in advance.

Pkm.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_ndru%2BGVShEMNnuFXURH301Y%3D8S3t68KOQNC%2Bf3HCq48EA%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...