Re: [MW:31886] Tubes expansion beyond drum thickness.

Any reference for expansion beyond drum thickness is not acceptable as per ASME Standards/IBR.


This is specifically mentioned in TEMA that expansion length shall be the tubesheet/drum thickness minus 1/8" (3.2 mm) and no expansion of tubes beyond drum/tubesheet thickness is acceptable.

However these standards are being followed for Heat exchangers (Heaters, condensers, coolers & re-boilers) only and our boiler is designed as per ASME Sec-1 and IBR.  


On Mon, Dec 28, 2020 at 10:37 AM Prasad Ghanekar <prsgne@gmail.com> wrote:
Expanded beyond shell thickness is not acceptable. There will be a notch formation on tube at edge of shell. Tubes are likely to be sheared at this point.

Prasad G.

On Sun, 27 Dec 2020, 10:31 Neeraj Yadav, <neeru25oct@gmail.com> wrote:

Min-8% to Max-20%
On Saturday, 26 December 2020 at 13:14:34 UTC+5:30 Vishwas Keskar Welding Manager WELDING wrote:
What is  expansion % ?


On Fri, Dec 25, 2020 at 3:57 PM Neeraj Yadav <neeru...@gmail.com> wrote:
Dear experts,

We are executing a project for 35 TPH Natural Gas fired Auxiliary Boiler designed for max. working pressure of 60 kg/cm2 and steam temperature of 392 Deg .Cel.

All water tubes of boiler are connected to steam( 63 mm Thk) & Mud drum(40mm Thk) with expanded design of construction.

In mud drum it is observed that tubes ( 51X4 mm) are expanded upto 30mm more than the drum thickness and indicating as bulged. we have checked the OD at bulged part and observed 1-2 mm flared and thickness around 3.5 mm

Kindly advise weather it is acceptable or we have to replace the se tubes with reference to code. Code of construction is ASME Sec-1/IBR.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bbc02a3f-f869-4c58-a898-ed522ce25df6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/16689637-a056-4dff-b3da-adacc1f9062bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3b2OP2nUAVO1Nk%2B1YSVdwMKCh%3DPLQKn1zD0HtDBYWO%2B5w%40mail.gmail.com.


--


Thanks & Regards


Neeraj Yadav

M.No.:+91-9457487464, 7017375440

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAHrL3F9nzm%3DB1MHOJpJYNxwB4k2pgniFFmv_U_%2BokVgEOu8Og%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...