Skip to main content

RE: [MW:31870] Subject:- Charpy Impact Testing on weld metal

U- Notch for Charpy impact tests used to be followed  DIN standards, back in 1970s. In fact DIN standards used to provide an option for both Notch types. Correlation of impact data was never easy.   It's discarded since then.

It's a matter of basic understanding : a V notch generates more stress than an U-Notch, Hence materials exhibiting good impact with V Notched specimens  would easily meet the criteria in U-Notch conditions not the other way. Notch toughness is an extremely critical property for engineering design.

Anything good under worse condition(V-Notch) is more reliable that something performed under ideal condition (U-Notch). Engineering codes, material properties  have matured  and improved leaps and bounds over the. Hence adoption of V-Notch Charpy impact test is an example of that principle.

Hope it clears your doubts.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Saudi Aramco Approved Designated Welding Engineer(DPWR)

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Shahil Saini
Sent: December 17, 2020 3:49 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:31868] Subject:- Charpy Impact Testing on weld metal

 

That I know sir, but I want some more information behind this topic why they discarded U notch and For every material they are not using U notch or for which materials U notch is used?

 

On Thu 17 Dec, 2020, 9:17 AM George Dilintas, <dilintas@gmail.com> wrote:

V notch simulation is more reliable 

 

Στις Τετ, 16 Δεκ 2020, 06:58 ο χρήστης Shahil Saini <sainishahil98@gmail.com> έγραψε:

Hello everyone, 

 

My question is, Why ASME BPVC and other standard codes discarded the 'U' notch impact testing?

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9KBo5H3LU6KOD1xU1LpWHVZwm5SJq4-Z%3DkQDprJTQTrw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DBBBfmR6sVKsFeL2w_g8SD3Hb1Tv3fu79ZK6TNi_1%3DCA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO__W5fmuqoj4BVvrg4%3DgUJfmFvtUVhG_JHNr5Av14QAAxg%40mail.gmail.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...