Skip to main content

Re: [MW:31811] WPS and PQR

NORMALLY IN API 1104 A CHANGE IN FILLER METAL TO ANOTHER IS ESSENTIAL VARRIABLE THAT NEED REQUALIFATION  

5.4.2.6 Filler Metal
The following changes in filler metal constitute essential variables:
a) a change from one filler metal group to another (see Table 1);
b) for materials with a SMYS greater than or equal to that of the material specified as API 5L Grade X65, a change in
the AWS classification of the filler metal (see 5.4.2.2).
Changes in filler metal within filler metal groups may be made within the material groups specified in 5.4.2.2. The
compatibility of the base material and the filler metal should be considered from the standpoint of mechanical
properties
  

Le jeu. 3 déc. 2020 à 09:07, 'Anumiah Veera Jegan' via Materials & Welding <materials-welding@googlegroups.com> a écrit :
Dear all,

The PQR and WPS for the project I am working on has multiple processes (GTAW for root and SMAW for fill and cap).Due to some constraints GTAW cannot be used. Can I use the same PQR and WPS to use SMAW for root , fill and cap as per API 1104 or do I need to requalify a PQR and WPS?. Thanks.

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fe75d6c2-bece-479f-8028-706fcd38ccc4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKdGSrpPLXg2oZEcEyP3uQOXvJckAu49pt%3DNMuyGv6Kgtw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...