Yes, if your PQR qualified on single test coupon, see QW-202.4 b) -2).

On Wednesday, October 21, 2020 at 9:12:59 PM UTC+7 Manish Kumar wrote:
Dear Sir,
If P number of material 1 & group number 1 & 2 is mentioned in WPS.While supporting relevant PQR is P number 1 & group number only 2. In this case,Will WPS be valid for relevant PQR.

Please advise us .

Attachment-
WPS & PQR 

--
Regards

Manish Kumar
Inspection(Mechanical) Engineer
PDIL-HURL Barauni site

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/897f0b27-a42f-4a0c-904a-0aade982b2f6n%40googlegroups.com.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...