At your place I would read carefully the Table UHA-32-1 is ASME BPVC Section VIII-1

Στις Τετ, 14 Οκτ 2020 στις 6:15 μ.μ., ο/η Vikas Bhandari <vikas.bhandari349@gmail.com> έγραψε:
Hi

I am looking to weld 410 wrought stainless steel, there is a requirement to build up parent material because of incorrect machining.

AWS A 5.9 ER410 is the filler wire.

Considering the carbon and Chromium content, looking for a preheat of 200°C with maximum interpass as 315°C.

I take it ,No interruption during welding will be good for joint. Material will be constantly maintained at the minimum preheat temperature during welding.

 

For post weld heat treatment , I am thinking of bringing the material to 100°C (This is to ensure that there is complete transformation of the weld and HAZ to martensite ) and then follow this with PWHT for 4 hours.

 

I am thinking of tempering temp of 610°C ( 20°C below tempering temperature of the material).

 

Any recommendation in this regard will be greatly appreciated.


Thanks & best regards


Vikas

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACpSjO%3Dnw0gymJLohpEzJ3aWuz7y462ASyMioCY3KnMWXHb7Fw%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Cgfsg41U7oLEdntXsOgwUCJLKM2v%2B0wefNbN%3DGd26%2BNg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...