Sunday, November 1, 2020

Re: [MW:31660] Allowable tolerance

Dear,

Refer referenced documents mentioned in applicable material specification.

Regards,
CH V RAMANA 

On Saturday, 31 October, 2020, 07:39:30 pm IST, Dhaneesh p <dhaneeshdotp@gmail.com> wrote:


Dear experts 
my query is , what is allowable tolerance in length , diameter , thickness for material receiving inspection of following ( please mention reference code   )
1) pipe ASTM 312 TP 304  , SIZE 3/4" , THK : 2.87 mm , Length : 6 m 
2) fittings  ASTM A 403 WP 304 , THK : 3.38
Regards 
Dhaneesh 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bda38b20-5a5b-4094-9d28-2b8a410fa53cn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...