Re: [MW:31754] Facing crack in during overlay welding of Stellite 12 on Duplex material


On Fri, 20 Nov 2020 at 15:16, SURESH <qms.pjgpl@gmail.com> wrote:
Dear Experts
During welding of Duplex grade material we are facing crack on the weld metal as attached in the photo. Below is the detailed process for reference

Process: PTAW
Base Material: ASTM 182 Gr.F55
Consumable: Stellite 12 (Powder)
PreHeat: Nil
Interpass: <200*C
Current: 128 to 145
Gas: Ultra Pure ARGON
Job Size: OD544 X ID 472 X Thk 36mm
Welding: Overlay weld on OD Surface alone


We are welding deposition thickness of 3mm. So as per this we are doing welding of 2 layer with multi pass, On welding second layer we found crack. Can anyone suggest where it is went wrong and why this crack is propagated. Please advice

 

In First layer- Total of 12 weld pass

In second layer- Total of 12 weld pass



Regards

Suresh

-

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmxsApjkzReQ9jjXkAweyx9tibcO2n5g2h8Qpt8pdKwEg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...