Re: [MW:31699] Preheat Requirements for in service pressure vessel ,

During the repair, you have to implement the same WPS used for production welds..
The depth of the repair may be smaller than the total weld thickness but the PWHT depends on the base metal thickness and not on the deposited metal thickness


Στις Τρί, 3 Νοε 2020 στις 5:51 π.μ., ο/η senthil vel <senthil7tlnd@gmail.com> έγραψε:
Dear Sir
As per design the vessel have no PWHT ,
During Repair Preheat Need?


On Mon, 2 Nov 2020, 14:30 NIKHIL THOMAS JOY, <nikhil.thomasjoy@gmail.com> wrote:

Dear experts,

Greetings of the day

I have a query related to the F Number in welding process.

IF I QUALIFY A WELDER WITH F No.6, He can weld all F.No-6.

But, if I Qualify with F No.5, can he weld F No.1 to 4.

Experts please reply as per code reference.

BEST REGARDS,
NIKHIL THOMAS JOY
IWI LIMITED 
ADNOC-WHRP
0544975526

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiVye%3DvWpXy28w6g%2Bvj77vUNNQHJGZp6dUUi%2Bb5aD1oyOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFVN5GE6m56XYQA-s%2BKFwFLj-GDkMRpB67aVC9VOfpW1bh4qxg%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D9Y8s07DBG8ahiQVEyTHgvjU52geP-FN%2BMFNKrWJ3Ynw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...