Does Diffusible Hydrogen test is applicable to AWS SFA 5.28 ER110S-G (Solid Wire) welding wire? As per the AWS 5.28 section, test should be done in accordance with AWS A4.3 section.
I have spoken with manufacturer of solid wires and as per their opinion Diffusible Hydrogen test is not applicable to any Solid wire grades.
Can any one clarify?
Regards,
Aditya Gujar
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c2c03ef1-fa2e-4d6e-b38a-efd28c4a02acn%40googlegroups.com.
Comments