[MW:31719] Re: electrode selection

I recommend the guideline >>> Welding Consumables guides in API RP 582 2016 - Welding Guidelines for the Chemical, Oil, and Gas Industries. Annex A: Table A.1 - Carbon and Low-alloy Steel

On Wednesday, October 28, 2020 at 2:55:16 PM UTC+7 QA/QC Deptt. TCPL wrote:
Please suggest electrode for welding sa516 & sa105

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/255045f6-048b-435c-988b-bc2d327dfe45n%40googlegroups.com.