Hi,
I think there're some mix-ups in the specifications and interpretations. SSPC SP6 or other specifications are applicable for surface preparation by blasting for application of paints.
For the refractories the criteria is a bit different. Following is the extract from API -936, for surface preparation before applications of refractory.
You may read the standard, discuss and settle the issue with the client based on the API-936 guidelines.
Thanks.
P.Goswami.P.Eng, IWE.
Independent & Consulting Welding & Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgoswami@rogers.com,pradip.goswami@gmail.com
Cell/Whasapp:1-905-9793232
From: RKD <raymondkenneth.dionisio@gmail.com>
Sent: November 26, 2020 10:15 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: SSPC SP 6 - 63
Hello everyone.
I encountered a requirement from a Licensor specification that internal surface should be prepared as per SSPC SP 6 - 63 prior to refractory application.
I know SSPC SP 6 means commercial blast but I have never encountered or saw a surface preparation requirement "SP 6 - 63".
Does anyone know what this means?
Thank you in advance.