Re: [MW:31699] WPS and PQR According to ASME Sec.IX and Sec.VIII- Boiler and Pressure Vessel Code

impact test requirements  when the Code of Construction is VIII-1 
You start from UG-20 Design Temperature to check for exceptions and then you go to UCS-65 & 66 & 67 in case of CArbon or Low Alloy Steel, not to forget UG-84 for test plates requirments

Στις Σάβ, 24 Οκτ 2020 στις 7:59 π.μ., ο/η K K <karan.hbl@gmail.com> έγραψε:
Dear Experts,

Please refer below WPS and PQR details.

PQR Details - Base Metal - ASTM A106 Gr.B  To ASTM A106 Gr.B. ( P No - 1 Gr.No - 1 To  P No - 1 Gr.No - 1 ).
Process - GTAW  + SMAW ( GTAW - 4.8 mm + SMAW - 13.46 mm)
Thickness of the Coupon -18.26 mm, Dia - 6"
With PWHT - 638°C ,time 72 min.
No Impact tested.
DESIGN TEMP. / MDMT (°C) -290 / 5 .

WPS Details - Base Metal - ASTM A106 / A516 Gr.B / Gr.70  To  ASTM A106 / A516 Gr.B / Gr.70 . ( P No - 1 Gr.No - 1/2 To  P No - 1 Gr.No - 1/2 ).
Process - GTAW  + SMAW ( GTAW - 9.6 mm + SMAW - 15.4 mm).
SFA No- GTAW - 5.18 and for SMAW - 5.1.
AWS No - GTAW - ER70S-3 and SMAW - E7018-1H4R.
Pre heat - less than 12.7 mm -10°C and less than 25 mm 75°C.
Inter pass Temp. -315°C.
PWHT - 620°C, Holding time 1 hr thk +1 hour min.

According to above details help me to review, as per ASME Section VIII for Boiler and Pressure Vessel Code.
And I need your suggestion what are the essentials requirements according ASME  Sec.VIII. And what are the important things i have to check.
Please suggested me with clause reference.

Please send me your valuable suggestions, it's Supports me lot.

Thanks and Regards
Kiran




 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c3e78183-f533-400b-bfe1-ba8e24f94c6an%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Dh5UDxVomGZhk%3DcYm%2B0z-6Abbac4VZPPna1ZzU2Mwhxw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...