[MW:31751] QUERY RELATED TO PWHT IN PQR & WPS

Dear Experts

Greetings of the day,

I Have an existing PQR of carbon steel P1G1 to P1G1 OF MATERIAL THICKNESS 21.94" & Diameter 6".

GTAW – 5.97mm & SMAW -17.1mm

PWHT – 640 deg. Cel. With soak time 75 min.

Impact test – Not Applicable

 

By using this PQR Can I make WPS for P1G1 to P1G1.Where T= 5mm to 25mm without PWHT (AS PER ASME B31.3  Para 331.1.1&331.1.3).

Because as per my project scope I need only 25mm maximum base metal thickness. So, for this I need to do PWHT or NOT. Although I have did PWHT in PQR.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96e00cdd-7b11-41ac-aa31-a2f39df5a5d9n%40googlegroups.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...