Thanks a lot. For the references 

On Tue, 3 Nov 2020 at 5:47 PM, George Dilintas <dilintas@gmail.com> wrote:
Read UW-40(e) and UCS-56(f).
The issue is too complicated to explain it in a mail

Στις Πέμ, 22 Οκτ 2020 στις 3:14 μ.μ., ο/η Zacharias Rohith Joseph <rohithjoseph18@gmail.com> έγραψε:
Hello, 
Can someone pls guide on how many times PWHT can be repeated on a weld and the requirement of PWHT for joint which have been repaired post PWHT. 

If there are references in other codes that you know of you may pls quote that too. 

Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/79e76538-eb77-4600-80d9-67389e9d72a1n%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/HTBZSGGULDY/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CO8Q5X5%2BGaWCC%2B2ipaB8Tvzq-1Ce4SW%2BA%2BRY5oO%3DVjYA%40mail.gmail.com.
--
With regards 
Zacharias Rohith Joseph 
9003939354

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKKFUw7qNQKU8w8cxkBgHjK%2BCDkMbitSNx7sbJjtAm5MWq7Lg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...