 Such a broad question. Let's start with this question. What code were you planning on qualifying to? Assuming ASME IX, Purchase yourself a copy if this is in fact the code you need to qualify to, and begin studying.
QW-451 For procedure qualification thickness limits and test specimens Should get you on the right track. I recommend getting in touch with somebody who is knowledgeable with creating a WPS/PQR. There's a lot more to it then what you asked in your question and what I've told you in my simple answer. More info is needed in order to help out.
Cheers......


On Mon, Nov 23, 2020 at 7:21 PM STEPHEN MESSIAH <qc42492@gmail.com> wrote:
How do we get thicknesses and materials for wps/pqr in a piping project? Is it from drawings or any other documents?

There could be thousands of drawings in a project.Is there a master document?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e53afe9e-8516-46f7-8572-46497cf0d053n%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUPQ-b0aDHdEuOTMG1MNQ%3Dx57KHYiS530hXS-kiwhDJhUA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...