Saturday, November 28, 2020

[MW:31785]

Dear All,

    Pls if any one have latest  C swipe 3.1 course study material .

Aslo pl. Date of Examination for C Swipe 3.1.

Pl. Do needful.

Thanks,
Ankit Patel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuwLMOVY5YFzrkCe%2BTzLmm11ET3%2B_f5G%2B6OZSKbRtJhk0A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...