--API RP 1102 Steel Pipelines Crossing Railroads and Highways
From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of sajeed zaheer
Sent: miércoles, 11 de noviembre de 2020 6:02 a. m.
To: materials-welding@googlegroups.com
Subject: Re: [MW:31730] pipeline crossing highway
Go through ASME 31.8 for gas transmission distribution piping system
On Wed, Nov 11, 2020 at 1:19 PM QA/QC <adnanziad49@gmail.com> wrote:
Dear experts
we are going to erect a new pipleline crossing a principal road with many cars and track of big load so what we can do to protect our pipe from big load anything from code and standards
can u help me
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4d25efc3-f435-4b4a-bb71-74d29665bf0bn%40googlegroups.com.--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMz4s%2BzLQdAeqzcyK603pfjHPrQDJPxuQNjGiPEg_YFe_w%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DB6PR04MB31761D36A972531E695A8D01E9E80%40DB6PR04MB3176.eurprd04.prod.outlook.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKeTQfqX3UUo_sFM2D4D88HkuqpCFZXTCJkeAbMfjfQ3%2BA%40mail.gmail.com.
Comments