Monday, November 16, 2020

Re: [MW:31744] Re: Imapct toughness testing on weld joint of material SA 516 Gr70

If your question is inquiring about were you can find UCS-66 and UG-84, seek out Boiler and Pressure Vessel Code, ASME Section VIII Division 1, Rules for construction of pressure vessels.
You can purchase the latest edition for the above mentioned at www.asme.org 
Cheers.....

On Sat, Nov 14, 2020 at 10:50 PM Shahil Saini <sainishahil98@gmail.com> wrote:
From where I get UCS-66 and UG-84?

On Thu 12 Nov, 2020, 9:15 AM Bien.ND |WIC, <bck055@gmail.com> wrote:
I agreed with Customer Care
Addition, I found problem in the PQR with actual test specimens that the subsize and reduction temperature not complied with UCS-66. You also check it out at UG-84.

On Tuesday, November 10, 2020 at 7:00:42 PM UTC+7 Shahil wrote:
Hello everyone, 
Can anyone help me in finding out problems arising during impact toughness testing of the weld joint of the pressure vessel.

Thank you,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1ad5e4df-0c79-4c0c-a88f-97248bf4aa9dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9koO8XgipLLcsrRWRiwDKei-TSpWomFNVmQ7%2Bo128oGA%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUPR7_ve0tJVzOjQNYyr-%2BgtGPNG15KRvf5a7YduTi4UeA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...