Re: [MW:31739] Diffusible Hydrogen Test for ER110S-G Welding wire

Manufacturer is correct.

On Fri, Nov 13, 2020 at 12:12 AM Aditya Gujar <gujar.adi@gmail.com> wrote:
Hello All,

Does Diffusible Hydrogen test is applicable to AWS SFA 5.28 ER110S-G (Solid Wire) welding wire? As per the AWS 5.28 section, test should be done in accordance with AWS A4.3 section. 

I have spoken with manufacturer of solid wires and as per their opinion Diffusible Hydrogen test is not applicable to any Solid wire grades. 

Can any one clarify?

Regards,

Aditya Gujar


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c2c03ef1-fa2e-4d6e-b38a-efd28c4a02acn%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUO26Cwv5YX0G0WXk3D16MyAQJS%3DCQzfC16sDGMSYj%3D9HA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...