The diffusible hydrogen test is "optional" per the specification.

 

The Annex provides a nice summary A8.2 (see below).  For high strength materials, it may well be prudent to require the diffusible hydrogen test to be performed to assure that the manufacturers product should not be a source for cracking.  Most often cracking issues are the result of improper low hydrogen controls during fabrication welding.  FYI - please note that I have experienced problems with bare wire contaminated with residual drawing compound in the past.  I expended considerable effort trying to find a local issue first before determining (and confirming) it was a wire manufacture issue. 

 

Enjoy. Stay well.

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Aditya Gujar
Sent: Friday, November 13, 2020 12:39 AM
To: Materials & Welding
Subject: [MW:31737] Diffusible Hydrogen Test for ER110S-G Welding wire

 

Hello All,

 

Does Diffusible Hydrogen test is applicable to AWS SFA 5.28 ER110S-G (Solid Wire) welding wire? As per the AWS 5.28 section, test should be done in accordance with AWS A4.3 section. 

 

I have spoken with manufacturer of solid wires and as per their opinion Diffusible Hydrogen test is not applicable to any Solid wire grades. 

 

Can any one clarify?

 

Regards,

 

Aditya Gujar

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c2c03ef1-fa2e-4d6e-b38a-efd28c4a02acn%40googlegroups.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...