Tuesday, November 3, 2020

[MW:31689] Cast iron to mild steel

Dear Expert, 

Good day.

I have to weld cast iron to mild steel.
What would be the suitable filler rod to use? 

Also is there any specific parameter or welding condition I have to follow since cast iron is difficult to weld. 

Example any specific heat treatment or post heating before welding? 

Kindly advice.

Best regards,
Pravin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7eaVq1UvD%2BgBxN8BiwjvxLoa4MSduXQisFPpOo4fRfStA%40mail.gmail.com.