Here are our procedure, you may refer to it.

Test medium

Test medium shall be cleaned or potable fresh water or rust inhibitor. Note that chloride content in water shall be less than 250 ppm for carbon steel components and chloride content in water shall be less than 50 ppm for stainless steel components.

Regards

Bien ND


On Friday, November 6, 2020 at 10:34:02 AM UTC+7 Nandush Sreekumar wrote:
what is the Commonly Recommend ph & Chloride Value for  hydro test Water For Cs & SS Materials 









NANDUSH.S

QC INSPECTOR

MKG GLOBAL LLC

DUQM REFINERY PROJECT-OMAN

MOBILE:968-79614049

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/11313a0f-cc1f-4f96-ae15-0962329e34can%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...