PH & PPM 

1 . C. S - less then 250ppm or specified by client spec. 
2. S.S- 50 ppm Or specified by client spec. 
3. PH - 07 natural water 6.5-7.5 best

Lesser PH value more acidic below 06 Or equivalent 06 for stainless steels, it's better to refer client specifications for PH value


Tejas

On Fri, 6 Nov, 2020, 9:03 AM Nandush Sreekumar, <nandush.s@mkgoman.com> wrote:
what is the Commonly Recommend ph & Chloride Value for  hydro test Water For Cs & SS Materials 









NANDUSH.S

QC INSPECTOR

MKG GLOBAL LLC

DUQM REFINERY PROJECT-OMAN

MOBILE:968-79614049

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e36293e0-a596-4488-a2b9-4c4ee5c3c2c4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACc1tDLSp-VpLOXMyPsgPwag23SXv3qJuNUNo5mwU7qRDgvBKw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...