dear 

check the pipe standard stenciled on the pipe for identification. It could be alloy steel pipe of  ASTM A 672 Grade A 45 etc......

Thanks & Regards,
Satyaprakash Soni,Manager - QA/QC,Mobile +91-9892649099


On Mon, Nov 30, 2020 at 3:30 PM RKD <raymondkenneth.dionisio@gmail.com> wrote:
Hi, I am no expert but have you checked the material certificate of this piping to confirm the process used?

On Thursday, November 26, 2020 at 12:17:23 PM UTC+8 faizul wrote:
    Dear Expert,

    I come across with 2" pipe line which having appearance like using auto-weld process.
    From my understanding, electric fusion weld should be no filler rod used. However, from the actual piping at site, the weldment seem to have weld cap and show obvious long-seam appearance.
    I am never across with small diam of pipe having
  • Question: How do we know if the welding is electric fusion process or not? I am never across with small diam of pipe having long-seam appearance from outside

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cfc63f2e-f4c7-4a99-89a9-c70e8395ed83n%40googlegroups.com.

****---------------------------**** 
Disclaimer : The information contained in this e-mail (including any attachments) is privileged and confidential. If you have received it by mistake please notify the sender by return e-mail and permanently delete this e-mail and any attachments from your system. Any dissemination, use, review, distribution, printing or copying of this message in whole or in part is strictly prohibited. Please note that e-mails are susceptible to change. Voltas Ltd. (including its group companies) shall not be liable for the improper or incomplete transmission of the information contained in this communication nor for any delay in its receipt or damage to your system. Voltas Ltd. (or its group companies) does not guarantee that the integrity of this communication has been maintained or that this communication is free of viruses, interceptions or interference.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB39JkDCn7CC0yVAvfHbHngkNU_vvRMr09Mar2FiQST6Ma1AbQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...