Re: [MW:31742] ph & Chloride Value for hydro test Water For Cs & SS Materials

Yes, code may not required, but project specification may require in the test package. I hope that everyone check in the specification also.

On Saturday, November 14, 2020 at 12:22:34 PM UTC+7 Patel Ankit wrote:
Dear Nandush,

Code dose not specified PH value for Hydro Test.
Pl. Ask to client and Testing according.

Regards,
Ankit Patel
QCE
 Chem Process system private Limited

On Fri 6 Nov, 2020, 9:03 AM Nandush Sreekumar, <nand...@mkgoman.com> wrote:
what is the Commonly Recommend ph & Chloride Value for  hydro test Water For Cs & SS Materials 









NANDUSH.S

QC INSPECTOR

MKG GLOBAL LLC

DUQM REFINERY PROJECT-OMAN

MOBILE:968-79614049

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e36293e0-a596-4488-a2b9-4c4ee5c3c2c4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5997fc22-ee08-4453-816c-0ee6bcebc7ffn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...