RE: [MW:31230] Combination of PQRs

Hello KK,

HIC testing usually does not apply or  procedure qualification according to Sec-IX or even  as per oil and gas industry standards, say NACE MR 103 , API(RP-582). Common industry document for HIC testing is NACE TM -0284, which calls for HIC testing on parent metals, plates/ pipes etc.

 

How does this idea of HIC testing originate? Is it possible for you to share any specific or relevant document?

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of K K
Sent: July 28, 2020 2:24 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:31226] Combination of PQRs

 

Hi,

 

Yes, Piping requirements.

 

SA 516 gr 60/70. and according to ASME Sec.IX and ASME B31.3.

The main PQR is qualified with PWHT, but not HIC tested.

And I have additional PQR with HIC tested, but not qualified with PWHT, and no other lab test reports like a mechanical test, bend test, and hardness test report, shall I combined this PQR to my WPS.

 

Please looking you feedback.

Thanks 

Kiran

 



On Tuesday, July 28, 2020 at 10:12:01 AM UTC+5:30, Sudhakar Kuppuswamy wrote:

Hi,

 

Please specify the material grade and the design code. 

 

As you have mentioned Line class, I presume you are talking about piping . 

 

Regards 

Sudhakar K 

 

On Mon, 27 Jul 2020 at 11:33 AM, K K <kara...@gmail.com> wrote:

Hi Experts,

 

"Good Morning"

 

According to my line classes, I required NACE+HIC+PWHT Wet H2 services.

What is the test shall be conducted according to the standard to meet the requirements?

 

I have one PQR with NACE+PWHT+Wet H2S services, but not HIC test.

In addition, I have qualified one HIC tested PQR without PWHT no other lab test certificates, shall I combined this PQR to the above requirements( NACE+HIC+PWHT+wet H2S).

For your information, the HIC test is an additional requirement of our specifications.

Please looking your feedback on my above query.

 

Thanks and Regards

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f1d53635-4e0f-4fe5-a0cf-ec93a8d2d87bo%40googlegroups.com.

--

Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhak...@gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/036721c7-5728-4727-b92a-ad48067f8453o%40googlegroups.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...