Skip to main content

Re: [MW:31212] SA 312 TP304 for SA 312 TP 304L

how to give purging for 3 meter dia shell to weld of SA316 Gr 240L material with GMAW (tig).

On Thursday, 16 July 2020 12:09:25 UTC+5:30, Dharma dattu wrote:
Thanks you all 

Question 1:  WPS was established in 2008, can it be used now?

Question 2: for a 3 meter dia tank how to give purging to do root weld with GTAW.

On Tuesday, 7 July 2020 12:19:39 UTC+5:30, Rajavarman wrote:
Hi.

Both are same P.no8/Group.no1.

So no issue to use the old WPS.
But must be consider,

1. Special requirements other essential variables such as thickness range, 
And supplimentry essential variables,
Based on particular project requirements.

2. Approval of new client.



என்à®±ுà®®் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Tue, Jul 7, 2020, 9:29 AM Dharma dattu <dharm...@gmail.com> wrote:
Hello All,

We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!

Regards,
Dharma Dattu. B

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/89ae66ad-2aad-40ce-aed3-fe009c801617o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/54b1da84-770d-4f2f-9553-a3a4cc4974f1o%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...