[MW:31141] Re: out of straightness tolerance for B31.3 piping


Hi u can refer the code - ASTM 999, where table no-2  shows the straight ness of piping.



On Saturday, April 23, 2011 at 1:22:24 PM UTC+5:30, Raj wrote:
Hi,

A 358 is specifies about variations in dimensions as mentioned below.
Refer 7.1.3 ??

7. Permissible Variations in Dimensions
7.1 Permissible Variations—The dimensions at any point in a length of
pipe shall not exceed the following:
7.1.1 Outside Diameter—Based on circumferential measurement, 60.5 % of
the specified outside diameter.
7.1.2 Out-of-Roundness—Difference between major and minor outside
diameters, 1 %.
7.1.3 Alignment—Using a 10-ft or 3-m straightedge placed so that both
ends are in contact with the pipe, 1⁄8in. [3 mm].
7.1.4 Thickness—The minimum wall thickness at any point in the pipe
shall not be more than 0.01 in. [0.3 mm] under the nominal thickness.

Other code A530 (Standard Specification for General Requirements for
Specialized Carbon and Alloy Steel Pipe) is specifies "Straightness
Tolerances" and mentioned in table-3. (But this is not applicable for
your case) - For your info only.

I just want to throw some light on your query !!!

Cheers!

Raj


On Apr 21, 3:30 pm, biju <biju....@gmail.com> wrote:
> Hi,
>
> We received some stainless steel pipes A358TP316L 16"SCH-10S having an
> out of straightness 23 to 25 mm .Pipe length is around
> 11.800mtrs.Client rejected those pipes.Is B31.3 saying any thing about
> out of straightness requirements. If their please provide me the
> details. Also is their any manufacturing spec requirements for this?
>
> regards,
>
> Biju

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a7dcd90b-8275-4e77-9d88-f4e7fa58362bo%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...