Re: [MW:31128] Suitability for wps

Correct shyam agree with you and also we need to incorporate the 3G PQR (impact tested) no.+2G PQR no. in the new WPS for 2G position.

On 10-Jul-2020, at 12:36 AM, Shyam Krishnan A P <shyamkrishnan7@gmail.com> wrote:

ear Chris,

In AWS D1.1 , Position is an essential variable for PQR(WPS). According to Table 6.1(of Ed 2020, Or in Table 4.1 of Ed 2015 ) , a PQR qualified in 2G will qualify for only F&H position and 3G  only for Vertical Position (Refer Table 6.19 of  Ed 2020).And hence you may need PQRs separately. Supplementary Impact test coupons may be prepared if you haven't  performed  Impact Test ( If you comply with all essential variables listed in Table 6.5 and Supplementary essential variables listed in table Table 6.7 of Ed 2020 ) to support existing PQR (refer Clause 6.26.3 of Ed 2020).

And  I think you were confused with Clause of AWS D1.1 Ed 2015 or earlier, Stated in Table 4.6 (Supplementary Essential variables for CVN application):          A change in position to vertical up. A 3G vertical up test qualifies for all positions and vertical down. Its very important to understand this clause also.This doesn't mean that a PQR tested in 3G position will qualify for all positions.Its meant that You need not Impact test (supplementary coupon) for a 2G PQR, If You have a PQR in 3G With Impact Tested Results provided, all Essential And Supplementary essential variables remains the same for Both PQR.ie You may use 2G PQR for Impact Applications even if You did not performed Impact test with help of 3G PQR .However even in Earlier editions of AWS D1.1 Production Positions qualified remains the same as that of Previous Paragraph.

Thanks & Regards

On Thursday, 9 July 2020 07:45:06 UTC+4, chris wrote:
Hi friends

I have made a wps in 3g as per AWS d1.1 , I was under the impression that if I qualify in 3g it will automatically be qualified for flat and horizontal.But it seems there is a code restriction for this and I can weld only 3g for production welds.
My doubt is if i make one more test coupon in 2g for the same wps and get it qualified will it work??
Or should I need to create a new wps jus for this 2g position ??

Thanks in advance
Chris

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/728e5755-b7f8-4892-bb81-62c6adeddf22o%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...