Re: [MW:30702] SS 317L welding with 316L consumable

308L filler can also be used . 

On Mon, 10 Feb 2020 at 12:46, Venkat <venkadesan86@gmail.com> wrote:
Hi experts

Contractor is proposing SS 316L pipe in place of SS 316L since it is not readily available (requirement is 20" pipe, 0.5m length with 2 nos joints). Though it is superior grade I am having doubt on welding. 
SS 316L PQR is already established with 316L welding filler wire and electrode. 

Can the same PQR be used in SS 317L pipe(thickness limits is within the WPS range)?  

Regards,

N. Venkadesan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c0ec4f17-27a7-490e-916e-4721e5f44e04%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OhnVXoG__8GAwG7Zkw5kzvT6Pom%3Dr2EK%3DcQStzg2GYf4Q%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...