Re: [MW:28872]

 If you maintained minimum test pressure  entire holding period test is accepted. 

Regarding needle valve- To be replaced / repair

Regards
MS Nair

On 8 Jan 2019 12:35 pm, "Nishanth Km" <nishanthkm21@gmail.com> wrote:
Dear experts,

Please advise

Hydro test conducted under Asme 31.3, after test duration time it was found the bleed valve in the the manifold found leaking.

Can we accept the test or reject? Please mention how also?

Regards


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...