[MW:28872] Interpretation: IX-10-23 Subject: QW-433 and QW-452.1(b) Date Issued: March 14, 2011 File: 10-1918

Greetings,

I have clarifications with below interpretaion for question 1 and agree with 2 and 3, does anyone has any observations on Q1?

Interpretation: IX-10-23 Subject: QW-433 and QW-452.1(b) Date Issued: March 14, 2011 File: 10-1918 
Background: A welder tests on an NPS 6 Sch. 80 (0.432 in. wall) coupon, depositing 0.100 in. of E6010 and the balance of 0.332 in. using E7018. Question (1): Using E6010, is the welder qualified to deposit 0.864 in. maximum of weld metal? Reply (1): Yes. Question (2): Using E7018, is the welder qualified to deposit 0.664 in. maximum of weld metal? Reply (2): Yes. Question (3): Is the welder qualified to deposit 0.864 in. of weld metal using E6010 plus 0.664 in. of E7018 weld metal deposit thickness for a total of 1.528 in. in the same groove? Reply (3): No. See QW-452.1(b).

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...