Tuesday, January 1, 2019

[MW:28836] Re: Thickness range for PQR

10 to 26mm

On Wednesday, November 14, 2018 at 1:44:24 PM UTC+3, Jibin Philip wrote:
Dear Experts..

code asme sec 9 ,B31.3 .. pqr test plate thickness is 20 mm ..need charpy test .. so what will be thickness range qualified ??
Regards,
Jibin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...