Hi,
If you check the parent material, you shall get major three elements of UNS8020 and the same with filler 625 checking the weldment.
Thanks.
  Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
"Whoever does not show mercy to the people, Allah will not show mercy to him." (Jami` at-Tirmidhi, Vol. 4, Book 1 / 1922)
Hello ExpertsWhat will be expected PMI result on weld done with filler wire 625 for joining material of uns8020.RegardsVikas P. Waghmare--https://materials-welding.blogspot.com/https://www.linkedin.com/groups/122787---You received this message because you are subscribed to the Google Groups "Materials & Welding" group.To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.Visit this group at https://groups.google.com/group/materials-welding.For more options, visit https://groups.google.com/d/optout.