Re: [MW:28749] TI To SS welding

Not advisable, you will definetly get cracks and brittleness easily.

Thanks.

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

"Whoever does not show mercy to the people, Allah will not show mercy to him." (Jami` at-Tirmidhi, Vol. 4, Book 1 / 1922) 

 
Date: 2018-12-11 12:59
Subject: [MW:28747] TI To SS welding
I have query about TI to SS welding. I have tubesheet of SS and Tube is Ti. One option is TUbesheet is cladded WITH Ti. But I want to know about TI to SS welding in this type of configuration.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...