Dear Mr Dinesh,

There is no doubt that the project specifications always governs. But I would recommend you to follow data sheet since it seems more stringent than PS.

Painting data sheet show RH 80% max based on the test performed by the manufacturer in laboratory under simulated conditions.
Also check for dew point, metal temperature & other manufacturer recommendations before proceeding.

Thanks & regards,
Jay Poojary
QA/QC ENGINEER
AWS- CWI
BGAS Level 2



On Mon, Dec 10, 2018, 12:03 PM Dinesh Somwanshi <som.din@gmail.com wrote:
Dear sir,

Please advice in following subject.

For painting, I have paint data sheet saying 80 % shall follow humidity while project specification says 85 % shall follows.

Which document shall be refer for Humidity either paint data sheet or project specification.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER


असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...