Wednesday, December 5, 2018

Re: [MW:28734] LR BEND TO LR BEND WELDING IN PIPELINE AS PER API1104

Nope dear, i just asking about LR Hot Bend welding.

On Wed, Dec 5, 2018 at 4:28 PM Anil Kumar <bathulaanilkumar@gmail.com> wrote:
I think  you are asking about cold bending operation, and welding of joints between two bend sections, it is allowed as,"extremities of each joint remain straight over a minimum distance of 2 m or twice the pipe diameter, whichever is greater" . this is referred from SP 1208 Pipeline Construction specification (PDO Specfication).

Thanks & Regards,

Bathula Anil Kumar

PH N0: +91-7675019922



On Wed, Dec 5, 2018 at 6:35 AM Mohit <mohitmechlion@gmail.com> wrote:
Dear all,

Can we perform welding directly LR Bend to LR Bend in pipeline ??

Refer to code API 1104.

Joint is before to IJ(Isolation Joint) at Intermediate Pigging Station.

Thanx in advance.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Mohit Kumar Singh
9687117556

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...