Thursday, December 27, 2018

[MW:28818] Material Testing queries.

Dear sir,

I needed advice,  along with Reference code for EIL specs Jobs.

a) I received plate from X mill, While verifying MTC it has been observed that 1 tensile test has been provided, While code requirements of 2 tensile test. 
How we can proceed for MTC approval with check test? ( either 1 additional test of Tensile or 2 tensile ) 

B) I received plate from X mill, While verifying MTC it has been observed that for 310S, content of MO missing in MTC as per code has requirement of MO . 
How we can validate to proceed for MTC approval with check test ?( either 1 chemical content of MO / full content chemical analysis / Both tensile  Chemical)  

Please Advice.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER


असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...