I need some clarification as below.

1)  GMAW Process WPS and PQR Qualified with  A36 -Group no- I. Can I mentioned in WQTR  range qualify with Group No-I,II,III and IV.

2) SMAW Process - Can I Mentioned In WPS range as what i Mentioned in table.


 PQR 

 

WPS range

1

Specification No

 A 5.1-04

 

A 5.1

2

AWS No

E-7018

 

E 6010 / E 7018

3

Filler No

4

 

1,2,.3,4

4

Analysis No

1

 

1

 

 

 

 

 

5

polarity

AC(+)

 

AC & DC

 
Please if any thing wrong please let me know with AWS D1.1 Standard.

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...