RE: [MW:27998] thickness qualified

Sec. IX ~ Maximum to be welded = Maximum thickness allowable for the code of construction.

For ASME B31.1 this is interpreted as unlimited thickness.

 

 

 

Thanks,

 

 

Chip Frizzell

Construction Manager

 

CWI / ASNT NDT Lvl III / NACE CIP Lvl 2 – Certified

 

chipfrizzell@gmail.com

CELL: 520-510-8093

 

Price is what you pay – Value is what you get.

Seldom does the lowest price result in the best value!

 

Integrity . Satety . Respect

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Joby Thomas
Sent: Thursday, June 28, 2018 5:46 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:27996] thickness qualified

 

Hi,

 

can any one of you guys clarify what is maximum to be welded ?

 

does it mean the welder can weld unlimited thickness?

thank you

On Tuesday, June 26, 2018 at 11:44:02 AM UTC+8, kannayeram gnanapandithan wrote:

For welder, deposited weld metal is essential. if you have welded 16mm butt joint with more than 3layers of deposition, he is qualified for max to be welded. Plate thickness is not essential for welder?


THANKS & BEST REGARDS,

KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

 

On Tue, Jun 26, 2018 at 8:57 AM, 'Raja kumarasamy' via Materials & Welding <material...@googlegroups.com> wrote:

Dear all,

 

Good morning

 

Could you please advise on this matter?

 

 

Sub-contractor welder qualified plate T: 16mm as per Sec IX. (maximum can be weld as per Table: QW-452.1(B)

 

shall he can be welded in a plate T: 10mm if possible, where is it mentioned in the Sec IX. Please….

 

 

 

Regards 

 

Raja kumarasamy

Welding & Piping inspector

Salalah LPG Project

Oman Gas Company (OGC)

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...