dear,

it,s composition match with 18- 8 grade near to about austonitic steels.

regards

On Thu, Jun 21, 2018 at 10:20 PM, <nithindsilva4u@gmail.com> wrote:
Yes you have to refer to Filler wire (SFA 5.9) chemistry.

Sent from my iPhone

On Jun 21, 2018, at 21:31, Abhishek Vyas <vyas121@gmail.com> wrote:

Hi,

Hope the attached picture helps you for chemistry of EQ309LMo.

Regards,
Abhishek Vyas
Welding Engineer
voestalpine Bohler Welding India

On Tuesday, May 8, 2018 at 12:59:20 PM UTC+5:30, anhtrang nghieng wrote:

Dear experts,

 

Can anyone give me Chemical Composition Requirement for EQ 309LMo . I could not find in ASME SFA-5.9/SFA-5.9M.

 

Thanks.

 

Gigi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
<Chemistry EQ309LMo.PNG>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...