Here group no. falling in supplimentary essential variable.Client is asking to perform above PQRs. Our intention is to do one PQR and thus prepare above 3 WPS . Can We?

On Thu, Jun 7, 2018, 08:13 Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
what you want to say on this. when there is impact requirement, group no is essential??

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Jun 5, 2018 at 8:15 PM, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
SEE ATTACHMENT

2018-06-05 1:02 GMT-05:00 JIJILAL K M <jijilalkm2@gmail.com>:
Dear Experts,

We are in requirement of PQR qualification for ASTM A106 Gr.B (ASME P1 G1)  with  ASTM A105  (ASME P1 G2) materials with notch toughness test as per ASME IX.

When PQR is qualified ,can we make following wps

P1G1 + P1G1
P1G1 + P1G2
P1G2 + P1G2   

If can, please advice which part of the code is agreeing with this.

Best Regards,
K M JIJILAL

+91 70346 35080
+91 98461 28141



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...