ASTM casting grades

CARBON STEEL AND CHROMES
WCB/WCC (Carbon)
LCB/LCC (Low Temp Carbon)
WC6 ( 1-1/4 Cr.)
WC9  (2-1/4 Cr.)
C5     ( 5 Cr.)
C12   ( 9Cr- 1Mo)
C12A (9Cr-1Mo-V)
300 SERIES STAINLESS
CF8M/CF3M (316/316L)
CF8/CF3 (304/304L)
CG8M/CG3M (317/317L)
CK20 (310)
CF8C (347)

ALLOY 20, DUPLEX and SUPER DUPLEX
CN7M (Alloy 20)
CN3MCu (Low C Alloy 20)
CN3MN (AL6XN)
CK3MCuN  (254-SMO)
CD3MN (Duplex 2205)
CE3MN (Super Duplex Gr. 5A)
CD3MWCuN (Super Duplex Gr. 6A)
CD4MCuN  (Super Duplex Gr. 1B)
INCONELS
CY40 (Inconel 600)
CW6MC (Inconel 625)
CT15C (Incoloy 800)
CU5MCuC (Inconel 825)
HASTELLOYS
N12MV (Hastelloy B)
N7M (Hastelloy B2)
CW12MW (Hastelloy C276)
CW6M (Hastelloy C Modified)
CX2MW (Hastelloy C22)
MONEL AND OTHER EXOTIC ALLOYS
M35-1 (Monel 400)
M30C (Weldable)
C-2, C-3 and C-7 (Titanium)
702C (Zirconium)
CZ100 (Nickel 200)