[MW:27766] Cracked Impeller Wear Rings

Dear experts,

Have several cracks on the wear rings of a Goulds pump Impeller.  PMI has been performed and rings have been identified as --17-4 Ph.  The impeller itself is a mild c/s.
Have no references on welding these two metals together?  Any ideas or procedures?

Respectfully,

Butch26

--