Dear Experts,

 

Have 17-4 Ph impeller wear rings welded to C/S impeller.  There are several cracks in the rings to be repaired.  What is the proper weld rod and procedure the weld these cracks?

 

 

 

Respectfully,

Butch Murrell

Coastal Machine & Mechanical,  LLC

Office: 979/849-9323

 

 

 

 

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone