Skip to main content

Re: [MW:27381] If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?

Dear sir,

Backing gas or Purging Gas is not essential variable for WPS.

Thank you

On Sun, Feb 25, 2018 at 10:39 AM, Peter Soloman <petervsoloman@gmail.com> wrote:

Just check the qualification details.  P8 to P8 qualifies for P1 to P1 also.  F number for carbon steel and stainless steel filler wire are same. But deletion of backing gas(QW 408.8) is an essential variable. Since you are not giving backing gas for CS, the welder cannot weld CS with GTAW even though he is qualified on SS with GTAW.   

And if the contractor wish the welder to weld CS where he is qualified on SS,  They can weld the joint by providing backing gas for CS, provided CS GTAW WPSs shall have backing gas mentioned in it.  But 99% of CS WPS for GTAW will not have backing gas!!!


 

Required welding variables as per Sec IX is below.  Hope this helps


Regards,
PETER SOLOMAN

On Sun, Feb 25, 2018 at 9:44 AM, 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Good morning everyone 

Sir you are write. 

For GTAW can not weld due to essential variables deletion of fas. 

Regards 
Anand gupta
Iocl  baroda


On Sun, 25 Feb 2018 at 8:38 AM, Amit Singh
Removal of Gas Backing is essential variable that's why a SS GTAW qualified welder is not qualified for CS GTAW joints, however reverse can be true for GTAW procedure only
Regards, 
Amit Singh

On 24-Feb-2018 18:30, "'Prashant Panchal' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Please check gas backing is essential variable for welder qualification. 
On Sat, Feb 24, 2018 at 6:23 PM, sankar rao
If welder qualified with SS 
(GTAW Process),
He can weld CS ( GTAW Process)
Because of F.No's same for both SS &CS  for GTAW 
SS ---- F.NO 6.  SFA NO. 5.9
CS----- F.NO 6.   SFA NO. 5.18

On 24 Feb 2018 14:50, "'Prashant Panchal' via Materials & Welding" <materials-welding@ googlegroups.com> wrote:
Since he may have used backing gas for SS gtaw he will not be qualified for carbon steel as we do not use backing gas for cs material. 
Alternatively u will have to use backing gas for cs as well


On Sat, Feb 24, 2018 at 3:33 PM, PK M
Dear Sir,

If a welder is qualified with SS (Stainless Steel) GTAW,  He can weld CS Carbon steel GTAW? Need code Referance...

Thanks.
PKM

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...