Skip to main content

Re: [MW:27307] What is the allowable inner penetration during pipe wedling

Dear Friend,

Thanks for your reply,

My doubt is How much height of weld metal can be allowed as inner penetration?since inner penetration clearly seen in RT film and reported, but end client is asking acceptable limit. Can you give?      

Regards,
Sankaran.SP
Welding & Metallurgy expert
Cell no: 9486409307


On Wednesday 31 January 2018, 5:31:06 PM IST, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


There are lot of Factors involved in Radiography to determine the Density Variation for the ID penetration depth. Moreover you use a Double wall viewing and it is very difficult to determine.

Other methods include

1. Boroscopy
2. Ball run Test. A steel ball with the required diameter shall be passed through the tubes and determine the depth of penetration.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Wednesday, January 31, 2018, 2:52:31 PM GMT+4, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Experts,

During pipe to pipe welding by single V butt joint by GTAW process (example : 1" XXS P91 pipe), there is a weld reinforcement over the groove and maintained 2 to3 mm of height, such a way ID penetration is also there. How much of height ID penetration is allowed? which is to be checked by RT exam. Kindly clarify and give me any supporting/ document  reference.

Regards, 

Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .